| Title: | Process for producing deep-drawing Low-carbon aluminium-killed steel based on CSP technology | ||
| Application Number: | 200610098396 | Application Date: | 2006.12.18 |
| Publication Number: | 1970809 | Publication Date: | 2007.05.30 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C22C38/06;B21B1/46;B21B37/74;B21B37/48;B21D5/00;C21D8/02;C21D11/00 | ||
| Applicant(s) Name: | Maanshan Iron | Address: | |
| Inventor(s) Name: | Zhang Jian;Liu Yonggang;Shen Chang;Yang Xingliang; | ||
| Attorney & Agent: | xuhui | ||
|
|
|
||
Abstract: |
|||
| The invention discloses a manufacturing method of deep-impaction low-carbon and aluminium killed steel board based on CSP technique, which comprises the following steps: smelting; casting thin board continuously; rolling; annealing at lid-type. The low-carbon smolten steel comprises the following parts: 0.01% | |||
|
|
|||
| Time: | 9 | ||