| The invention discloses a mill run technology of bauxite, especially relates to a ore wash-floatation technology of cumulate bauxite. For cumulate bauxite, changing the single ore wash technology into ore wash and appending dispersant, and floatation to the gangue. The invention can increase the quality of wash-concentrate and decrease the mud ratio of wash-concentrate; by floatation, a number of gibbsite, diasporite, bodhmite can be reclaimed, achieve the intention of using bauxite. | |||
|
|
|||
| Time: | 12 | ||
<- Previous Patent:Equipmiment for collecting liquid...
| Next Patent:Flotation method for sulfidizatio... ->
|
|||