| Title: | Technological method of iron removal of nepheline ore by strong magnetic concentration | ||
| Application Number: | 200510022343 | Application Date: | 2005.12.21 |
| Publication Number: | 1785529 | Publication Date: | 2006.06.14 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | B03C1/30,B03B7/00 | ||
| Applicant(s) Name: | Nanjiang Minerals Development Co. Ltd., Sichuan Pr | Address: | 636600 |
| Inventor(s) Name: | Yue Juncong, Qin Yuanxiang | ||
| Attorney & Agent: | liu shiquan | ||
|
|
|
||
Abstract: |
|||
| A process for removing iron from nepheline ore includes such steps as crushing nepheline ore grinding, sieving to divide the ore powder into (30-100)-mesh class and (80-200)-mesh class, strong magnetic wet separation for (30-100)-mesh class, strong magnetic dry separation for (80-200)-mesh class, and packing. Its recovery rate of ore concentrate is increased to more than 70%. | |||
|
|
|||
| Time: | 15 | ||