| Title: | Multicomponent copermeation process using boron-rare earth salt bath | ||
| Application Number: | 85100311 | Application Date: | 1985.04.01 |
| Publication Number: | 1002000 | Publication Date: | 1986.07.30 |
| Approval Pub. Date: | Granted Pub. Date: | 1987.06.24 | |
| International Classifi-cation: | C23C12/02 | ||
| Applicant(s) Name: | Shenyang Mechano-Electrical College | Address: | |
| Inventor(s) Name: | |||
| Attorney & Agent: | HUANG YUJIE | ||
|
|
|
||
Abstract: |
|||
| In order to overcome defect of brittleness of the boronisation layer,boron-rare earth-silicon ternary co-permeation process is adopted in this invention and rare earth-silicon alloy is used as reducing agent. Salt bath temp. was adjusted by sodium chloride additive for improving abrasion resistance, high temp. Oxidation resistance and corrosion resistance of the work piece. | |||
|
|
|||
| Time: | 2 | ||
<- Previous Patent:Diamond surface metallization tec...