| Title: | Material for thermal spraying and its method | ||
| Application Number: | 85101453 | Application Date: | 1985.04.01 |
| Publication Number: | 1007091 | Publication Date: | 1987.01.17 |
| Approval Pub. Date: | Granted Pub. Date: | 1990.12.05 | |
| International Classifi-cation: | B22F9/08,C23C4/06 | ||
| Applicant(s) Name: | Castolin S.A. | Address: | |
| Inventor(s) Name: | Hans-Theo Steine | ||
| Attorney & Agent: | WU DAJIAN LUO HONG | ||
|
|
|
||
Abstract: |
|||
| This material consists of following molten metals (wt. percentages): Cr:10-30 Al:1-25 C:less 0.5 Ni: less 10 Fe: remains To powder this material for thermal spraying, the cooling rate is more than 400 deg.C/s., the graininess of the powder is 27-150 microns, specific surface is more than 500 cm2/g. The powder can be thermo-sprayed on metal-body to form a coating whose strength is more than 20 N/mm2. | |||
|
|
|||
| Time: | 10 | ||
<- Previous Patent:Alloy pre-coating process of Sn-A...
| Next Patent:Chemical nickel plating process f... ->
|
|||