| Title: | Releasing tin metal in high lead low tin alloy and apparatus therefor | ||
| Application Number: | 85102241 | Application Date: | 1985.04.01 |
| Publication Number: | 1007180 | Publication Date: | 1987.01.17 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C22B13/10,C22C3/00,C22C11/06,C22C13/00 | ||
| Applicant(s) Name: | Research Inst. of Yunnan Tin Co. | Address: | |
| Inventor(s) Name: | Huang Rongkai, Huang Weisen, Lin Heqing | ||
| Attorney & Agent: | |||
|
|
|
||
Abstract: |
|||
| In the electrical heating, continuous crystallizing furnace through the temp. gradient within furnace formed from the electrical heating and the slope of the crystallizing furnace installation, and under the action of spiral device, different compositions of soldering tin and raw lead can be produced from the said alloy. | |||
|
|
|||