| Title: | Low iron loss cold-rolled orientation silicon steel plate (containing 4 Percent of Si) and its preparation method | ||
| Application Number: | 85100666 | Application Date: | 1985.04.01 |
| Publication Number: | 1002320 | Publication Date: | 1986.08.13 |
| Approval Pub. Date: | Granted Pub. Date: | 1987.07.01 | |
| International Classifi-cation: | C21D8/12,C22C38/26,H01F1/16 | ||
| Applicant(s) Name: | Central Research Inst. of Iron | Address: | |
| Inventor(s) Name: | Li Jun, Li Junyi, Liu Zhifu, Lu Qichun | ||
| Attorney & Agent: | CHENG GUANGHU | ||
|
|
|
||
Abstract: |
|||
| Besides adjusting the amount of main components such as C, Mn, and S etc., of a 4% Si steel, ALN is added as an auxiliary inhibitor. By controlling hot-rolling temp., improving heat-treatment in hot-rolling and preheating steel to 40-100 deg.C. before cold-rolling, the silicon steel plate of 0.35 mm. thick with iron loss of P15/50 is less than 0.9w/kg and orientation (110)[001] is produced by ordinary twice cold-rollings and intermidiate annealing processes. | |||
|
|
|||
| Time: | 7 | ||