| Title: | Method of maintaining steady coal-water slurry | ||
| Application Number: | 87101684 | Application Date: | 1987.03.05 |
| Publication Number: | 1016794 | Publication Date: | 1988.03.02 |
| Approval Pub. Date: | 1993.03.03 | Granted Pub. Date: | 1993.03.03 |
| International Classifi-cation: | C10L1/32 | ||
| Applicant(s) Name: | Hitachi Ltd. | Address: | |
| Inventor(s) Name: | Hideo Kikuike;Kiyoshi Muranaka;Takaichi Kaji | ||
| Attorney & Agent: | FAN BENGUO | ||
|
|
|
||
Abstract: |
|||
| This invention relates to a method of maintaining the viscosity of the slurry low and stable without deteriorating the properties thereof during the storage over a long period of time by adding alkali metal silicate and/or carbonate capable of forming a water insoluble compound with ions of calcium and/or magnesium to the slurry. The amount of the alkali metal silicate and/or carbonate should be sufficient to maintain the concentration of the ions to a predetermined level by converting the ions to the insoluble compound, and controlled by detecting dissolved ions of calcium and/or magnesium in the supernatant of the slurry, continuously or intermittently. | |||
|
|
|||
| Time: | 9 | ||