| Title: | Heating method for transporting bulk asphalt | ||
| Application Number: | 98102856 | Application Date: | 1998.07.14 |
| Publication Number: | 1241614 | Publication Date: | 2000.01.19 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C10C3/10 | ||
| Applicant(s) Name: | Zhonghai International Trade Group Corp., Ltd. | Address: | 200080 |
| Inventor(s) Name: | Yao Yongsheng | ||
| Attorney & Agent: | yan jufen | ||
|
|
|
||
Abstract: |
|||
| The present invention relates to liquid transportation, and features that the asphalt transporting method adopts separated heating equipment and heat exchange equipment, that is, the transported asphalt is heat held only without being heated on the way and is heated fast to 160 deg.c through connecting the hinged joint on arriving the unloading place before unloading. | |||
|
|
|||
| Time: | 7 | ||