Abstract:
     Rubber asphalt modifier is prepared with waste rubber bits and residual oil Materials including waste rubber 50-85 wt% and residual oil 15-50 wt% are reacted at 250-300 deg.C inside a reactor for 6-12 hr and the product is cooled in air to obtain the modifier. The raw materials for the modifier and discards, so that the modifier is low in cost and power-saving. The modifier is added asphalt to improve its quality.