| Title: | Storage stable modified asphalt and its preparing mehtod | ||
| Application Number: | 00123512 | Application Date: | 2000.08.18 |
| Publication Number: | 1339556 | Publication Date: | 2002.03.13 |
| Approval Pub. Date: | Granted Pub. Date: | 2003.04.30 | |
| International Classifi-cation: | C08L95/00,C10C3/02 | ||
| Applicant(s) Name: | China Petrochemical Corp. | Address: | 100029 |
| Inventor(s) Name: | Guo Shuhua, Huang Weiqi | ||
| Attorney & Agent: | xu shu | ||
|
|
|
||
Abstract: |
|||
| The storage stable modified asphalt is prepared with the material including asphalt 50-97.7 wt%, polymer 2.0-20.0 wt%, compatilizer 0.1-20.0 wt%, coupling agent 0.1-10.0 wt% and polar compound 0.1-10.0 wt%l, and through mixing and reaction at 100-250 deg.c for 5-300 min. It has excellent storage stability and softening point difference of isolation test lower than 2.5 deg.c. The preparation process of the present invention is simple and needs no special equipment. | |||
|
|
|||
| Time: | 8 | ||
<- Previous Patent:Preparation of interphase carbon ...
| Next Patent:Process for preparing modified as... ->
|
|||