| Title: | Inner wall epoxy phenolic aldehyde paint and its prodn. method | ||
| Application Number: | 96115319 | Application Date: | 1996.05.17 |
| Publication Number: | 1165844 | Publication Date: | 1997.11.26 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C09D163/00 | ||
| Applicant(s) Name: | Sun Xiuxiang | Address: | 150001 |
| Inventor(s) Name: | |||
| Attorney & Agent: | LI CHANGCHUN | ||
|
|
|
||
Abstract: |
|||
| A paint for food containers is prepared through mixing ethyl acetate, butyl acetate, cyclohaxanone, butanol and toluene, heating, addition of phenolic resin, heating while stirring, addition of epoxy resin, high-temp stirring, cooling, addition of dibutylester, acetone and titanium oxide powder, stirring and grinding to obtain particles with 20-25 microns of size, and features low cost and easy construction. | |||
|
|
|||
| Time: | 10 | ||
<- Previous Patent:Solid altering appliance