| Title: | Thick slurry type of epoxide coal bituminous coating | ||
| Application Number: | 85103608 | Application Date: | 1985.05.17 |
| Publication Number: | 1000162 | Publication Date: | 1985.12.20 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C08L63/00,C09D5/08,C09L95/00 | ||
| Applicant(s) Name: | Scientific Inst. of Pipeline, Ministry of Petroleu | Address: | |
| Inventor(s) Name: | Wang Jianfu, Wang Yizhu, Yang Fujun, Zhang Dong, Z | ||
| Attorney & Agent: | MENG QINGQUAN | ||
|
|
|
||
Abstract: |
|||
| The cpds. and the proportions of the ground coat may comprise the following ingredients: epoxide resin 15-30%, anthracene oil 20-40%, iron oxid red 20-40%, zinc chrome yellow 2-15%, mixed solvent 5-25%.The cpds and proportions of top coat include following: epoxide resin 10-35%, anthracene oil 10-30%, coal bituminous 10-30%, talc powder 5-20%, mica powder 5-20%, mixed solvent 5-20%, levelling agent 1-5%. Coats of the invention have short terms of drying, high machanical strength, good adhesive power, acid-resistance, base-resistance. They are applied at nomal temp. to renew or repair the anti-corrosive layer of pipeline without interruption of transportation. | |||
|
|
|||
| Time: | 7 | ||