| Title: | Process for preparing silane crosslinked polyethylene by room temperature crosslinking | ||
| Application Number: | 200610052520 | Application Date: | 2006.07.18 |
| Publication Number: | 1900130 | Publication Date: | 2007.01.24 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C08F255/02;C08K5/5425 | ||
| Applicant(s) Name: | Zhejiang Polytechnic Univ. | Address: | |
| Inventor(s) Name: | Wu Runde;Tong Xiaoli | ||
| Attorney & Agent: | huang meijuan yuan muji | ||
|
|
|
||
Abstract: |
|||
| The present invention is room temperature cross-linking process of preparing silane cross-linked polyethylene, and the silane cross-linked polyethylene is prepared with grafting material and catalytic material in the weight ratio of 5-20 to 1 and through room temperature cross-linking. The grafting material consists of polyethylene resin 100 weight portions, alkenyl alkoxy silane 0.5-5 weight portions, alkyl trimethoxy silane 0.5-3 weight portions, titanium-alkoxide chelate 0.5-3 weight portions and free radical initiator 0.01-2 weight portions. The catalytic material consists of polyethylene resin 100 weight portions, water generating agent 0.5-30 weight portions, cross-linking catalyst 1-5 weight portions. Compared with available technology, the present invention has the features of advanced technological process, high product yield, low power consumption, excellent product performance, etc. | |||
|
|
|||
| Time: | 4 | ||