| Title: | Modified halogen butyl rubber and processing | ||
| Application Number: | 85108409 | Application Date: | 1985.11.20 |
| Publication Number: | 1011209 | Publication Date: | 1987.05.27 |
| Approval Pub. Date: | Granted Pub. Date: | ||
| International Classifi-cation: | C08C19/10 | ||
| Applicant(s) Name: | Exxon Res | Address: | |
| Inventor(s) Name: | |||
| Attorney & Agent: | WANG JIE ZHANG YUANZHONG | ||
|
|
|
||
Abstract: |
|||
| The content of conjugated diene in the polymer is lower than 0.25% mole and the halogen is at least lower than 0.6% by weight. At leasl 20% mole of the halogen is presented as primary allyl form in the polymer. Said modified hologen butyl rubber is using Friedel-crafts or HBr as catalyst to be prepd. by traditional halogen butyl rubber isomerization. | |||
|
|
|||